phil99
 Guru
 Joined: 11/02/2018 Location: AustraliaPosts: 3319 |
| Posted: 06:55am 04 Oct 2023 |
|
|
|
Have had success reviving a DHT11 in a jar with some silica gel (salvaged from many pill bottles) and sitting it on the wood heater for a few hours. The AHT10 datasheet says 10 hours at 80 - 85 C.
Two addresses are available so 2 can use the same I2C. A solder bridge at the top selects the alternate - &H39. Edited 2023-10-04 17:04 by phil99 |